Abstract

Remanit 4404 is an 18 Cr-8 Ni + molybdenum type corrosion-resistant stainless steel that offers decreased carbide precipitation, and has good resistance to acids. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-698. Producer or source: Thyssen Stahl AG.