Abstract

Märker G 4857W is a cast alloy for petrochemical applications such as furnace tubes. It compares favorably to the HP Modified grades. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: Ni-512. Producer or source: Schmidt & Clemens Edelstahlwerke.