Abstract

Colmonoy No. 705 is a nickel-base corrosion and abrasion resistant atomized and crushed powder. It is enriched to the highest extent in tungsten carbide for maximum metal-to-metal wear resistance. Hardness 58 to 63 HRX is reached. This datasheet provides information on composition, physical properties, microstructure, and hardness. It also includes information on joining and powder metal forms.Filing Code: Ni-506. Producer or source: Wall Colmonoy Corporation.