Abstract

Sandvik Sanicro 41 is an austenitic nickel-base alloy with excellent resistance to reducing acids, has better pitting resistance than Type 316SS, and has excellent resistance to stress-corrosion in chlorides and downhole environments. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-505. Producer or source: Sandvik.