Abstract

VDM LC-Nickel 99.2 is unalloyed nickel which offers excellent corrosion resistance in many alkaline media. The metal also has good mechanical, magnetic, and magnetostrictive properties. It has a reduced carbon content to avoid graphitization at temperatures above 570 deg F (300 deg C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-502. Producer or source: VDM Technologies Corporation.