Abstract

Ni-Rod Filler Metal 44 is a solid, nickel-iron-manganese wire designed for automatic and semiautomatic welding of ductile, malleable, and gray cast irons in all positions. NI-Rod Filler Metal 44 offers high-speed, high-quality welds and can be used with all robotics, automatic, and semiautomatic processes, in all positions. A key advantage is the capability of welding all types of cast iron to steel and even stainless steel. This datasheet provides information on composition and tensile properties. It also includes information on joining. Filing Code: FE-114. Producer or source: Inco Alloys International Inc.