Inco-Weld Filler Metal 686CPT is a welding product with higher (Cr + Mo + W) content than most other nickel-base welding products. This higher alloy content increases the resistance to pitting, crevice, and general corrosion. Applications include welding many CRA materials for corrosive service. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on joining. Filing Code: Ni-517. Producer or source: Inco Alloys International Inc.