Precision C is a heat-treatable nickel-iron alloy used in critical diaphragm applications. The alloy composition provides a unique constant elastic modulus value over a temperature range of -50 to 150 deg F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: FE-113. Producer or source: Hamilton Precision Metals Inc.