Abstract

Tribaloy alloy T-900 is a cobalt-base alloy derived from an alloy family originally developed by DuPont. Excessive amounts of molybdenum and silicon induce the formatin during solidification of a hard and corrosion-resistant intermetallic coumpound, known as Laves phase. This alloy had improved crack resistance and a lower preheat temperature compared with Tribaloy T-800 (Alloy Digest Co-99, September 1996). This datasheet provides information on composition, microstructure, and hardness. It also includes information on corrosion and wear resistance. Filing Code: CO-100. Producer or source: Stoody Deloro Stellite Inc.