Abstract

MAERKER G4827 is an iron-chromium-nickel-silicon corrosion and heat resisting casting useful to 11 C (2102 F) in air. This datasheet provides information on composition and physical properties. It also includes information on casting and joining. Filing Code: SS-603. Producer or source: Schmidt & Clemens Inc.