Abstract

BioDur TrimRite Stainless has a composition that is balanced to be fully martensitic in the hardened condition. The alloy possesses a moderately high level of corrosion resistance and is applied as valve parts, guides, shafting and cutlery, including surgical tools. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating and machining. Filing Code: SS-599. Producer or source: Carpenter.