SANDVIK SANICRO 70 is an austenitic alloy with good high temperature resistance to carburization and nitridation. The alloy is also very resistant to chloride-ion stress-corrosion cracking and to hydrogen chloride. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: Ni-483. Producer or source: Sandvik.