VANADIS 10 is a chromium-molybdenum-vanadium powder metallurgical cold work tool steel offering a combination of extremely high wear resistance and good toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on wear resistance as well as heat treating. Filing Code: TS-536. Producer or source: Uddeholm Corporation.