Abstract
TYPE 316L-SCQ stainless steel is a cleaner version of AISI Type 316L. The clean microstructure, a reduction in the frequency and severity of non-metallic inclusions, allows a better electroplated surface. The unique applications considered for this microstructurally clean alloy include the semiconductor market to maintain gas purity. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: SS-587. Producer or source: Carpenter Technology Corporation.