ZERON 25 is an alloy developed to combat severe oil field duties where oil, gas, water are contaminated with high levels of chlorides and hydrogen sulfide. The alloy has good mechanical strength and resistance to localized corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-584. Producer or source: Weir Material Services Ltd.