VLX 562 is a high-strength austenitic-ferritic alloy with superior resistance than most 300 series stainless steels to stress-corrosion cracking. It is used in fresh water, where chlorides are present, and in high pressure applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-583. Producer or source: Vallourec Inc.