Abstract
Allegheny Ludlum Type 201 covered here (see also Alloy Digest SS-616, October 1995) is a modified composition (0.03% max C) for low temperature and heavy section service) This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on low temperature performance. Filing Code: SS-624. Producer or source: Allegheny Ludlum Corporation.