Abstract

Nimofer 6928 is a corrosion resistant solid solution 28Mo-Nickel alloy with significant resistance to reducing environments, particularly hydrochloric, phosphoric and sulfuric acids. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-494. Producer or source: VDM Technologies Corporation.