Abstract

Sandvik 8R30 is an austenitic, titanium-stabilized stainless chromium-nickel steel. It is suitable for wet-corrosive service, but also has good mechanical strength at high temperatures. For applications requiring enhanced creep strength, it is recommended that the variant Sandvik 8R30H be used. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-622. Producer or source: Sandvik.