Abstract

CRUCIBLE CSM 21 is a high quality stainless mold steel for the plastics industry. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating, machining, joining, and surface treatment. Filing Code: SS-620. Producer or source: Crucible Service Centers.