Abstract

MAERKER G-4848 is a heat resistant alloy for the petro chemical industry. The alloy has very good creep-rupture strength with low embrittlement. Similar to HK Mod. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on casting and joining. Filing Code: SS-617. Producer or source: Schmidt & Clemens Inc.