REMANIT 4003 possesses good workability, weldability and is mainly used in the transportation industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-615. Producer or source: Thyssen Stahl AG.