Sandvik SANMAC 316L is a molybdenum-alloyed austenitic chromium-nickel steel with improved machinability. As compared to ordinary 316L it also has a higher molybdenum content. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, and deformation. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-614. Producer or source: Sandvik Steel Company.