Abstract
NILOMAG ALLOY 77 is a 77 Ni soft magnetic alloy with a high level of initial permeability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating. Filing Code: Ni-488. Producer or source: Inco Alloys International Inc.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
You do not currently have access to this content.