NICROBRAZ 170 is an extra high strength at high temperature braze filler metal. It is good for brazing nickel-base materials containing cobalt, tungsten, and molybdenum. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-476. Producer or source: Wall Colmonoy Corporation.