Abstract
HASTELLOY B-3 ALLOY is a nickel-molybdenum alloy with thermal stability to reduce the deleterious intermetallic precipitates which cause loss of ductility and corrosion resistance. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance. Filing Code: Ni-461. Producer or source: Haynes International Inc.