Abstract

Developed in 1990, Fast-Cut 20 and 45 steels are available in those two nominal carbon levels and provide the highest level of machinability because of their elevated sulfur levels. This datasheet provides information on composition, and microstructure. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-131. Producer or source: Lukens Steel Company.