NICROBRAZ LM is a low melting general-purpose brazing filter metal for applications requiring high joint strength and oxidation resistance up to 2200 F. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-452. Producer or source: Wall Colmonoy Corporation.