CHROME CORE 8 AND 8-FM alloys are controlled chemistry alloys for use in magnetic components where better corrosion resistance than iron and steel alloys is needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SA-473. Producer or source: Carpenter.