NICROBRAZ 150 is excellent for jet engine parts and similar highly stressed components. It has good strength at lower brazing temperatures. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-469. Producer or source: Wall Colmonoy Corporation.