Abstract

NICROBRAZ 130 is a good general-purpose filler metal. It flows freely in marginal atmospheres, in deep or tight joints. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-468. Producer or source: Wall Colmonoy Corporation.