Abstract

COPPER ALLOY NO. C72900 is a spinodal alloy that develops exceptionally high elastic strength levels; dimensional stability and relaxation resistance at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: CU-588. Producer or source: Copper and copper alloy mills.