AMPCO-TRODE 160 is an aluminum bronze coated electrode that produces deposits with a good combination of strength, ductility and hardness. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-584. Producer or source: Ampco Metal Inc.