Abstract

COLMONOY NO. 88 is a nickel-based hard-surfacing alloy with bimetallic carbides for maximum wear resistance. This datasheet provides information on composition, physical properties, and hardness. It also includes information on machining and powder metal forms. Filing Code: Ni-429. Producer or source: Wall Colmonoy Corporation.