Abstract

WAUKESHA METAL NO. 23 is a nickel-base casting alloy having high resistance to corrosion, good machinability, and freedom from any tendency to seize or gall. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance, corrosion and wear resistance as well as machining and joining. Filing Code: Ni-49. Producer or source: Waukesha Foundry Company. Originally published January 1959, revised March 1993.