AMPCO-TRODE 10 is the most versatile aluminum bronze welding electrode in its family and is used for both similar and dissimilar welding. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining. Filing Code: CU-582. Producer or source: Ampco Metal Inc.