Abstract

CARPENTER GLASS SEALING 42 has wide-ranging applications in glass-to-metal and ceramic-to-metal sealing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining, and surface treatment. Filing Code: FE-102. Producer or source: Carpenter.