Abstract

AMPCO-TRODE 250 is used in extreme bearing applications and to weld AMPCO 21 castings (See Alloy Digest Cu-93, October 1960). This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-591. Producer or source: Ampco Metal Inc.

This content is only available as a PDF.
You do not currently have access to this content.