Abstract
THYRAPID 3341 is similar to AISI M2, but adds sulfur. It is general purpose high-speed tool steel with good toughness, red hardness, and excellent machinability. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-512. Producer or source: Thyssen Specialty Steels Inc..