NITRONIC 30 is a nitrogen-strengthened stainless steel with a good combination of strength, corrosion and wet abrasive wear resistance and economy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, and deformation. It also includes information on corrosion and wear resistance as well as forming, heat treating, and joining. Filing Code: SS-533. Producer or source: Armco Advanced Materials Corporation.