ZYAZIRC Z105 and ZYAZIRC Z328 are zirconias that are respectively stabilized with 10.5 and 12% yttria. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and compressive and bend strength. Filing Code: Cer-12. Producer or source: Vesuvius McDanel.