CMSX-2 is a single crystal alloy development of Cannon-Muskegon Corporation designed to achieve a high level of balanced properties. This datasheet provides information on composition, physical properties, as well ascreep and fatigue. Filing Code: Ni-417. Producer or source: Cannon-Muskegon Corporation.