CM 247 LC alloy is a derivative of the MAR M 247 composition, specifically designed for directionally solidified (DS) turbine blade and vane applications. This datasheet provides information on composition and physical properties. It also includes information on casting and heat treating. Filing Code: Ni-415. Producer or source: Cannon-Muskegon Corporation.