ZYALOX MV30 and ZYALOX MV20 are mullites combining low thermal expansion, good mechanical strength and resilience at elevated temperatures. This datasheet provides information on composition, physical properties, microstructure, elasticity, tensile properties, and compressive and bend strength as well as fracture toughness. Filing Code: Cer-10. Producer or source: Vesuvius McDanel.