Abstract

ALLVAC 6A1-6V-2Sn is a highly beta stabilized alpha + beta titanium alloy, a modification of the 6 A1-4V system. Added vanadium plus copper and iron produce the stabilizing effect. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-98. Producer or source: Teledyne Allvac.