Aluminum Alloy 383.1 is a controlled copper content aluminum die casting alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance. Filing Code: Al-318. Producer or source: Aluminum Smelting and Refining Company Inc..