TACTIX 556 is a multifunctional epoxy novolac resin. Its dicyclopentadiene structure has extremely low average molecular polarity, a feature critical to low moisture absorbance. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: P-26. Producer or source: The Dow Chemical Company, Dow Plastics.