NIMONIC ALLOY 105 is a wrought nickel-cobalt-chromium-base alloy strengthened by additions of molybdenum, aluminum and titanium. It has been developed for service up to 950 C (1742 F). This datasheet provides information on composition, physical properties, and elasticity as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-66. Producer or source: Inco Alloys International Inc.. Originally published August 1961, revised May 1991.