Copper Alloy No. C27400 is a high-zinc, yellow brass with excellent cold formability. It has excellent soldering and brazing characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: Cu-560. Producer or source: Copper and copper alloy mills.