Abstract
ASP 23 is a high-speed tool steel manufactured by the ASP powder metallurgy process in which the steel is atomized, compacted, and hot formed to the desired dimensions. This datasheet provides information on composition, physical properties, hardness, elasticity, and bend strength. It also includes information on heat treating, machining, and joining. Filing Code: TS-503. Producer or source: Uddeholm Corporation.